Oddy Test Results for 5 samples of Polyolefin 2:1 heat-shrink tubing as follows:

TEST PROCEDURE: Oddy

An Oddy test was conducted on five samples of polyolefin tubing. The test procedure was as follows: Each sample of polyolefin was enclosed in a separate glass vial with blanks of polished lead, silver and copper.  Half of the sample was placed beneath the blanks so that any effect of direct contact as well as volatile contaminates could be assessed.  Moist cotton was placed in the test vial, which was then sealed and exposed to 55ºC for 35 days.  

A control vial was prepared in the same manner, without any sample, and exposed to the same conditions.   

DAY

SAMPLE NUMBER

 

 OBSERVATION

1-35

Sample 1:
1/16"diameter

34-121

No change in test blanks. 

1-35

Sample 2:
1/8"diameter

34-122

No change in test blanks. 

1-35

Sample 3:
3/16"diameter

34-123

No change in test blanks. 

1-35

Sample 4:
1/4"diameter

34-124

No change in test blanks. 

1-35

Sample 5:
3/8"diameter

34-125

No change in test blanks. 

1-35

Control

No change in test blanks. 


Requested by Benchmark, Rosemont, N.J. 08556